Alloy C-2000, UNS N06200

Chemical composition % Ni Cr Mo Fe Co C Mn Si P S Cu Al min balance 22.0 15.0 1.3 max 24.0 17.0 3.0 2.0 0.010 0.50 0.08 0.025 0.010 1.9 0.50 Physical properties Density 8.50 g/cm3 Melting range 1328-1358°C Features Alloy C-2000 is a versatile corrosion-resistant alloy with excellent resistance to uniform […]
Alloy G-35, UNS N06035

Chemical composition % Ni Cr Fe Mo W Co C Mn Si P S Cu Nb+Ta min balance 28.0 13.0 4.0 1.5 1.0 0.30 max 31.5 17.0 6.0 4.0 5.0 0.030 1.5 0.80 0.040 0.020 2.4 1.50 Physical properties Density 8.22 g/cm3 Melting range 1370-1400°C Features Alloy G-35 is a high-chromium nickel-base alloy […]
Alloy S, UNS N06635

Chemical composition % Ni Cr Mo Fe Co W C Mn Si P S Al Cu La B min balance 14.5 14.0 0.30 0.20 0.10 0.01 max 17.0 16.5 3.0 2.0 1.00 0.020 1.00 0.75 0.020 0.015 0.50 0.35 0.10 0.015 Physical properties Density 8.75 g/cm3 Melting range 1335-1380°C Features Alloy S has […]
Alloy 230, UNS N06230

Chemical composition % Ni Cr W Mo Co Fe C Mn Si P S Al La B min balance 20.0 13.0 1.0 0.05 0.30 0.25 0.20 0.005 max 24.0 15.0 3.0 5.0 3.0 0.15 1.00 0.75 0.030 0.015 0.50 0.050 0.015 Physical properties Density 8.97 g/cm3 Melting range 1301-1371℃ Features Alloy 230 combines […]
Alloy X750, UNS N07750

Chemical composition % Ni Cr Fe C Mn Si S Ti Nb+Ta Al Co Cu min 70.0 14.0 5.0 2.25 0.70 0.40 max 17.0 9.0 0.08 1.00 0.50 0.010 2.75 1.20 1.00 1.00 0.50 Physical properties Density 8.28 g/cm3 Melting range 1393-1427°C Features Alloy X750 is an age-hardenable nickel-chromium alloy with good corrosion […]
Alloy 617, UNS N06617

Chemical composition % Ni Cr Co Mo Fe C Mn Si S Al Ti Cu B min 44.5 20.0 10.0 8.0 0.05 0.80 max 24.0 15.0 10.0 3.0 0.15 1.00 1.00 0.015 1.50 0.60 0.50 0.006 Physical properties Density 8.36 g/cm3 Melting range 1330-1375℃ Features Alloy 617 has excellent resistance to oxidation and […]